Sandvik 7C27Mo2 medical strip

Strip steelDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Sandvik 7C27Mo2 is a martensitic stainless chromium steel alloyed with molybdenum, supplied in strip form. It is mainly supplied in hardened and tempered condition, characterized by:

  • Very high corrosion resistance
  • High toughness
  • Excellent fatigue strength properties.

Sandvik 7C27Mo2 can also be supplied in soft condition, annealed or cold rolled for good formability.

Standards

  • : S42026

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.