Sandvik 7C27Mo2

Strip steelDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 7C27Mo2 is a martensitic stainless steel alloyed with molybdenum that is characterized by good formability. After hardening, the grade has:

  • Very good corrosion resistance
  • High toughness
  • Excellent fatigue strength

Sandvik 7C27Mo2 is typically used for cutters in electric shavers and springs.

Standards

  • : S42026
  • : (1.4031)*

*) Nearest equivalent grade

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.