Sandvik SAF 2507®

Strip steelDatablad

Datablad opdateret 2021-09-23 06:18 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik SAF 2507® is a super-duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. The grade is characterized by:

  • Excellent resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • Very high mechanical strength
  • Physical properties that offer design advantages
  • High resistance to erosion corrosion and corrosion fatigue
  • Good weldability

Standards

  • : S32750
  • : 1.4410
  • : X 2 CrNiMoN 25-7-4

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.