Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 3207 HD™ is a hyper-duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions where also high mechanical strength is necessary. This makes the grade ideal for applications such as deepwater umbilicals. SAF 3207 HD™ is characterized by:

  • Excellent resistance to pitting and crevice corrosion
  • Excellent resistance to stress corrosion cracking (SCC) in hydrogen sulphide (H2S) and chloride containing environments
  • High resistance to general corrosion in acidic and caustic environments
  • Excellent resistance to erosion corrosion
  • Excellent corrosion fatigue properties
  • Exceptionally high mechanical strength
  • Exceptionally high fatigue strength
  • Physical properties that offer design advantages
  • Good weldability

Standards

  • : S33207

Product standards

Seamless tube and pipe: ASTM A789; A790

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.