Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 253 MA is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterized by:

  • High creep strength
  • Very good resistance to isothermal and, particularly, cyclic oxidation
  • Good structural stability at high temperatures
  • Good weldability
  • Maximum operating temperature is approx. 1150°C (2100°F)

Trademark information: 253 MA is a trademark owned by Outokumpu OY

Standards

  • : S30815
  • : 1.4835
  • : (1.4893)*/(1.4828 mod.)*
  • : 2368*

Product standards

  • ASTM A213, A312
  • EN 10297-2
  • SS 14 23 68*

* Obsolete. Replaced by EN.

Approvals

Approved for use in ASME Boiler and Pressure Vessel Code, Section I, III and VIII, Div. 1 (SA-182, SA-213, SA-240, SA-249 SA-312 and SA-479).

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.