Sandvik 5R10

Tube and pipe, seamlessDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 5R10 is an austenitic chromium-nickel steel with a controlled carbon content in order to obtain improved strength at high temperatures.

Standards

  • : TP304, TP304H
  • : S30400, S30409
  • : 1.4301, 1.4948
  • : X5CrNi18-10, X6CrNi18-10
  • : 1.4301
  • : X 5 CrNi 18 10
  • : 2333
  • : Z 6 CN 18.09
  • : 304S31, 304S51
  • : SUS304TP

Product standards
Seamless tube and pipe

  • ASTM A271 and A376
  • JIS G3459
  • JIS G3463
  • EN 10216-5
  • BS 3605, BS 3606
  • DIN 17456, 17458
  • NFA 49-117, 49-217
  • SS 14 23 33

Approval
JIS Approval for Stainless Steel Tubes

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.