Sandvik Ti Grade 16

Tube and pipe, seamlessDatablad

Datablad opdateret 2021-07-12 12:49 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Ti Grade 16 is an unalloyed titanium grade with standard oxygen content and addition of palladium (0.04–0.08%).

Standards

  • : Grade 16
  • : R52402

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.