Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Ti Grade 2 is a Commercially Pure (CP) titanium seamless tubing characterized by:

  • Excellent resistance to general corrosion in seawater
  • Resistant to stress corrosion cracking in chloride and sour gas environments
  • Excellent resistance to pitting, crevice, and erosion corrosion
  • High heat transfer efficiency
  • Good formability and weldability
  • Very low thermal expansion
  • Moderate strength

Standards

  • : Grade 2
  • : R50400

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.