Sanicro® 48 for OCTG

Tube and pipe, seamlessDatablad

Datablad opdateret 2020-12-17 13:54 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 48 is an austenitic nickel-base alloy for highly corrosive OCTG downhole applications. The grade is characterized by:

  • Excellent resistance to sulfide stress cracking and stress corrosion cracking (SCC) in chloride and sour (H2S/Cl) environments
  • Very high resistance to pitting and crevice corrosion

Standards

  • : N06985

Product standards

Seamless tubes used as casing, tubing and coupling stock: ISO 13680, PSL-1 and PSL-2
API spec 5CRA

Approvals

  • NACE MR0175/ISO 15156-3 (Petroleum and natural gas industries - Materials for use in H2S-containing environments in oil and gas production)
  • Sanicro® 48, grade 110 ksi and grade 125 ksi, can be delivered with API-5CRA Monogram (License Number 5CRA-0016)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.