Sanicro® 61

Tube and pipe, seamlessDatablad

Datablad opdateret 2020-12-10 06:47 (afløser alle tidligere versioner)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 61 is a nickel-chromium alloy characterized by:

  • Good strength at high temperatures
  • Excellent resistance to high temperature corrosion, particularly in oxidizing conditions

The alloy is suitable for a wide range of applications where resistance to both heat and corrosion is a requirement.

Standards

  • : N06601

Product standards

  • ASTM B167
  • ASME SB167 

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.