Exera® 5R10/2R25 medical wire

WireDatablad

Datablad opdateret 2021-02-02 15:43 (afløser alle tidligere versioner)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Exera® 5R10 and Exera® 2R25 are austenitic chromium-nickel stainless steels. Exera® 2R25 is a low carbon version of Exera® 5R10. The grades are characterized by:

  • Good corrosion resistance
  • Excellent toughness
  • Good welding characteristics

Standards

  • : 304, 304L
  • : S30400, S30403
  • : 1.4301, 1.4306
  • : X5CrNi18-10, X2CrNi19-11
  • : 1.4301, 1.4306
  • : X5 CrNi 18 10, X2 CrNi 19 11
  • : 2332, 2352
  • : Z6 CN 18 09, Z3 CN 18 10
  • : 304S31

Product standards

  • ASTM F899
  • ISO 16061

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.