Our knife steels

Our program includes knife steel for all types of knives. Our knife steel is used in, for example, kitchen knives, chef's knives, fishermen's knives, hunting knives, folding knives and different types of industrial knives.
Vil du vide mere?
Every our knife steel has its benefits, ranging from excellent corrosion resistance to extreme hardness. The application determines the requirements of the knife. Choose a knife steel for your particular application and read more about its specific benefits.
Sandvik knife steels
- 14C28N - Combination of hardness and corrosion resistance
- 7C27Mo2 – High corrosion resistance
- 12C27 – The well-rounded knife steel
- 12C27M – Dish washer safe
- 13C26 – Razor edge sharpness
- 19C27 – Excellent wear resistance
- 10C28Mo2
- 10C16Mo3V1
* For electric shavers
Material selection table
Type of knife /application | 6C27 | 7C27Mo2 | 12C27 | 12C27M | 13C26 | 14C28N | 19C27 |
10C16Mo3V1 | 10C28Mo2 |
---|---|---|---|---|---|---|---|---|---|
Bread knives | - | - |
■
|
- | - | - | - | - | - |
Butcher's knives | - | - |
■
|
- | - | - | - | - | ■ |
Carpet knives | - | - | - | - | ■ | - |
■
|
■
|
-
|
Carving knives | - | - |
■
|
- | - | - | - | - | - |
Chef's knives | - | - |
■
|
- | - | ■ | - | - | ■ |
Circular knives |
■
|
■
|
■
|
■
|
■
|
- | - | - | - |
Cutting heads* | ■ | - | - | - |
■
|
- | - | - | - |
Fishermen's knives | - |
■
|
■
|
- | - | ■ | - | - | ■ |
Folding knives | - | - |
■
|
- | - |
■
|
- | - | ■ |
Frying slicers (spatulas) | ■ | - | - | - | - | - | - | - | - |
Hunting knives | - | - |
■
|
- | - | - | - | - | ■ |
Ice drills | - | - |
■
|
- | - | - | - | - | - |
Industrial knives | - |
■
|
- | - |
■
|
- |
■
|
■
|
-
|
Kitchen knives | - | - |
■
|
■
|
- | - | - | - | ■ |
Paper knives | - | - | - | - |
■
|
- | ■ | - | - |
Plastic film knives | - | - | - | - | ■ | - | ■ | - | - |
Pocket knives | - | - |
■
|
- | - | ■ | - | - | ■ |
Pruning shears | - | - |
■
|
- | - | - | - | ■ | - |
Shaver knives* | - |
■
|
- | - | - | - | - | - | - |
Skate blades | - | - |
■
|
- | - | - | - | - | - |
Surgical knives | - | - | - | - | ■ | - | - | - | - |
Synthetic fibre knives | - | - | - | - |
■
|
- |
■
|
-
|
-
|
Trimmers* | ■ | - | - | - |
■
|
- | - | - | - |
* For electric shavers