Welded pipe in sizes according to ASTM/ASME
Stainless welded pipe in sizes according to ASTM/ASME. Pipe is supplied annealed and pickled in random lengths or cut to fixed lengths in steel grades ASTM 304L and 316L. Welded pipes are either 100% Eddy Current tested or hydrostatic and expansion tested.
Vil du vide mere?
Available online
This product can be ordered online via our self-service platform E-Track, where you can also see stocks, get prices and view your order history.
E-Track is currently available in selected European countries but we are working on expanding the availability.
Stock program
Pipe is stocked according to ASTM A312/ASME SA 312, ASTM A999/M
Tolerances according to ASME B36.19.
OD = outside diameter, WT = wall thickness.
OD mm |
WT mm |
Nominal size | Weight, kg/m | 304L | 316L |
---|---|---|---|---|---|
21.34 | 2.11 | 1/2" SCH 10S | 1.02 | • | • |
21.34 | 2.77 | 1/2" SCH 40S | 1.29 | • | • |
26.67 | 2.11 | 3/4" SCH 10S | 1.30 | • | • |
26.67 | 2.87 | 3/4" SCH 40S | 1.71 | • | • |
33.40 | 1.65 | 1" SCH 5S | 1.31 | • | • |
33.40 | 2.77 | 1" SCH 10S | 2.13 | • | • |
33.40 | 3.38 | 1" SCH 40S | 2.54 | • | • |
42.16 | 1.65 | 1 1/4" SCH 5S | 1.67 | • | • |
42.16 | 2.77 | 1 1/4" SCH 10S | 2.73 | • | • |
42.16 | 3.56 | 1 1/4" SCH 40s | 3.44 | • | • |
48.26 | 1.65 | 1 1/2" SCH 5S | 1.92 | • | • |
48.26 | 2.77 | 1 1/2" SCH 10S | 3.16 | • | • |
48.26 | 3.68 | 1 1/2" SCH 40S | 5.49 | • | • |
60.33 | 1.65 | 2" SCH 5S | 2.42 | • | • |
60.33 | 2.77 | 2" SCH 10S | 3.99 | • | • |
60.33 | 3.91 | 2" SCH 40S | 5.52 | • | • |
73 | 3.05 | 2 1/2" SCH 10s | 5.35 | • | • |
73 | 5.16 | 2 1/2" SCH 40S | 8.77 | • | • |
88.90 | 2.11 | 3" SCH 5S | 4.58 | • | • |
88.90 | 3.05 | 3" SCH 10S | 6.56 | • | • |
88.90 | 5.49 | 3" SCH 40S | 11.47 | • | • |
101.60 | 3.05 | 3 1/2" SCH 10s | 7.53 | • | • |
114.30 | 2.11 | 4" SCH 5S | 5.93 | • | • |
114.30 | 3.05 | 4" SCH 10S | 8.50 | • | • |
114.30 | 6.02 | 4" SCH 40S | 16.32 | • | • |
141.3 | 3.4 | 5" SCH 10S | 11.74 | • | • |
141.3 | 6.55 | 5" SCH 40S | 22.1 | • | • |
168.3 | 2.77 | 6" SCH 5S | 11.48 | • | • |
168.3 | 3.4 | 6" SCH 10S | 14.04 | • | • |
168.3 | 7.11 | 6" SCH 40S | 28.69 | • | • |
219.1 | 2.77 | 8" SCH 5S | 15.0 | • | • |
219.1 | 3.76 | 8" SCH 10S | 20.27 | • | • |
219.1 | 8.18 | 8" SCH 40S | 43.2 | • | • |
273 | 3.40 | 10" SCH 5S | 22.95 | • | • |
273 | 4.19 | 10" SCH 10S | 28.2 | • | • |
273 | 9.27 | 10" SCH 40S | 61.22 | • | • |
323.9 | 3.96 | 12" SCH 5S | 31.72 | • | • |
323.9 | 4.57 | 12" SCH 10S | 36.54 | • | • |
323.9 | 9.53 | 12" SCH 40S | 75.02 | • | • |
355.6 | 4.78 | 14" SCH 10S | 41.99 | • | • |
355.6 | 9.53 | 14" SCH STD | 82.583 | • | |
406.4 | 9.53 | 16" SCH STD | 94.706 | • | |
406.4 | 4.78 | 16" SCH 10S | 48.07 | • | • |
457.2 | 4.78 | 18" SCH 10S | 54.151 | • | • |
508.0 | 5.54 | 20" SCH 10S | 69.702 | • | • |
610.0 | 6.35 | *24" SCH 10S | 95.919 | • | • |
*24" is produced with two seams