Capillary tubes

Capillary tubes with a maximum bore of 0.0158 in., available in a wide range of stainless steels. Sandvik capillary tubes are characterized by tight tolerances, and the inside surface of the tubes is free from oil, grease and other particles. This ensures, for example, an optimized and even flow of liquids and gases from the sensor to the measuring instrument.
Vil du vide mere?
Sandvik capillary tubes are used in applications, such as:
- Chromatography
- Gas and liquid lines
- Measurement components in remote thermometer systems (with or without compensation)
Typical sizes for Sandvik capillary tubes:
Outside diameter (mm) | Wall thickness (mm) | Inside diameter (mm) |
---|---|---|
2.00 | 0.95 | 0.10 |
2.50 | 1.21 | 0.08 |
3.00 | 1.40 | 0.20 |