Fine wire in a wide range of stainless steels and nickel alloys including resistance and resistance heating alloys. Sandvik's fine wire is available in sizes ranging down to 10 microns.
The fine wire is supplied in round or shaped form and is delivered with or without insulation and coating. Sandvik's fine wire is typically used in applications, such as:
- Precision measurement
transducers
- Precision resistors
- Temperature-stable
potentiometers
- Resistance thermometers
- Resistors, thermostat bars
- Self regulating heating elements
- Soldering irons
- Specialty filters
- Strain gauges
- Temperature compensating devices
- Temperature controllers
- Temperature probes
- temperature sensitive resistors
- Temperature sensors (PTC)
- Thermistor leads
- Temperature stable electronic
components
- Tolerances: Standard Limits,
or Special Limits
- Transducers
- Fuses
|
- Shunts
- Defrosters
- industrial infrared dryers
- Industrial rheostats
- Low temperature heating applications
- Lead wires
- Testing and automatic control equipment
- Timing devices
- Detonators
- Electric motor starter resistances
- Elements embedded in ceramics for panel heaters, in cartridge elements in metal dies
- Floor heaters
- Heaters and heating elements
- Heating cables
- Electric blankets
- High accuracy transducers
- High current resistors
- High value resistors and potentiometers for automotive and consumer electronics
- Appliances
- Hot plates, grills, toaster ovens, space heaters
- Igniters
- Heating cables and rope heaters
- Speaker coils
- Voice coils
- RF Coils etc
|
Fine wire insulation and coating
Sandvik offers several types of coatings including PTFE coating and adhesive bondcoats for its fine wire, all available in multiple colors.
For insulation and bondable coatings of fine wire Sandvik uses a continuous 'flood coating' process. The 'flood coating' process gives the wire quality and performance benefits over other techniques applied for fine wire, as 'flood coating' guarantees a complete coating over the wire surface, which is both consistent and extremely tenacious.
Read more about our insulation and coating capabilities