04. Martensitic Stainless Steels

Martensite, the hardest structural component in steels, is responsible for the high hardness in many sharp edge tools. The formation of martensite is a remarkable phenomenon in materials science and smiths have known for at least 3000 years how to make use of it to produce implements such as

04. Molybdenum and tungsten in duplex steels

In my previous column, I promised to give an overview of the role of molybdenum and tungsten in duplex stainless steels (DSS). They are neighbors of chromium in the periodic table (Group 6B) and even more potent than chromium in preventing pitting, which is shown in the familiar PRE-relation:

History specials

Episode 1. Göransson and Bessemer Read summary Episode 2. A new factory and a new town Read summary Episode 3. Bankruptcy and beyond Read summary Ep1 iframe Göran Fredrik Göransson, born in Gävle in 1819, joins Elfstrand’s, the trading firm his father manages and eventually becomes

03. Bankruptcy and beyond

Bankruptcy and beyond Fredrik had perfected the Bessemer process and built both a new factory in Sandviken and a functioning municipality which included a school for worker’s children. But huge loans and too little income in the end proved too much for the new company and both Högbo Iron and

02. A new factory and a new town

A new factory and a new town The year was 1858 and Fredrik Göransson struggled to build a new company and experimented with the Bessemer process. By July he had succeeded in stabilizing the process and took off for Hamburg with samples, thereafter to London to once again meet with Sir

01. Göransson and Bessemer

Göransson and Bessemer Göran Fredrik Göransson (called Fredrik by his family), founder of Sandvik in 1862, was born in the town of Gävle on the coast of the Baltic Sea, in 1819. The Göransson family was quite prominent in Gävle as Fredrik’s father was the manager of

Specials

Special: ASTM Award of Merit goes to Keith Hottle Special: Renewable energy Read the article Spc Kieth Hottle iframe Spc Renewable energy iframe

Renewable Energy

From the few examples mentioned in this column, new methods of generating electricity will also require new materials solutions to deal with the environments they will work in.

01. Austenitic stainless steels - from kitchen sinks to fuel cell cars

This column is the first in a series of eight columns on the topic of the seven families of stainless steels; their characteristics, complementary properties and the astonishingly wide variety of applications ranging from tiny stents in the human body to large scale constructions in the process

03. Duplex stainless steels- an interplay between ferrite and austenite

Number three in a series of eight columns throughout 2017 on the topic of the seven families of stainless steels; their characteristics, complementary properties and the wide variety of applications from the smallest of items destined for the human body to large scale constructions in the