Hier können Sie Materialdatenblätter für unsere breite Palette von Legierungen und Werkstoffen abrufen. Kontaktieren Sie uns, wenn Sie weitere Informationen zu unseren Werkstoffen benötigen.
Datenblatt anzeigen für:
UNS N08825 | ASTM 825, Alloy 825
A nickel alloy characterized by very good resistance to stress corrosion cracking in chloride and sour (H2S/Cl-) environments and very good resistance to corrosion resistance in acidic media such as sulphuric acid.
Mehrere Produktformen erhältlich:
Standard:UNS S32906 | EN number 1.4477
A high-alloy duplex (austenitic-ferritic) stainless steel with very good resistance in caustic environments and environments with chlorides.
Standard:UNS S21900
Sandvik 21-6-9 is an austenitic grade with a high level of Mn, a low level of Ni and the addition of N. The grade is characterized by:
Standard:
A thermoplastic polyamide.
A class 180 polyurethane coating.
A polyurethane wire enamel with additional Polyamide overcoat.
A Polyamide-imide insulation.
Standard:UNS N08904 | ASTM '904L' | EN number 1.4539
A vacuum arc-remelted high-alloy austenitic stainless steel with very high cleanliness resulting in good polishability. The grade is also characterized by very good overall corrosion resistance.
Standard:UNS S30400, S30403 | ASTM TP304, TP304L | EN number 1.4301, 1.4306
An austenitic stainless steel with a low carbon content. The grade is part of the Sandvik Bioline medical materials range.
Standard:UNS S32304 | EN number 1.4362
A lean duplex (austenitic-ferritic) stainless steel characterized by high resistance to stress corrosion cracking, good resistance to pitting and general corrosion and high mechanical strength.
Gehe zu Seite: Zurück , 1 , 2 , 3(Diese Seite) , 4 , 5 , 6 , 7 , … , 20 Weiter