High-temperature tubes - stock program
Sandvik holds stock of five different grades commonly used in a variety of high-temperature tube applications. Our tubes are used as, for example:
- Boiler tubes (reheater and superheater tubes)
- Furnace rollers
- Lance tubes
- Muffle tubes
- Pigtails
- Recuperator tubes
- Thermocouple protection tubes
We also offer composite tubes from stock.
Sandvik grade | UNS | ASTM | EN |
---|---|---|---|
Sandvik 4C54 | S44600 | 446-1 | 1.4749 |
Sandvik 7RE10 | S31008/S31009 | 310S, 310H | 1.4845 |
Sandvik 253 MA* | S30815 | - | 1.4835 |
Sandvik 353 MA* | S35315 | - | 1.4854 |
Sanicro 31HT | N08811/N08810 | - | 1.4959 |
* 253 MA and 353 MA are trademarks owned by Outokumpu Stainless.
Stock program
OD = outside diameter
■ = cold worked, □ = hot worked
OD mm |
WT mm |
Nominal size | Kg/m | Sandvik 4C54 |
Sandvik 253 MA |
Sandvik 353 MA |
Sanicro 31HT |
Sandvik 7RE10 |
---|---|---|---|---|---|---|---|---|
17.15 | 2.31 | 3/8 Sch 40S | 0.858 |
■*
|
■
|
- | - |
■
|
17.15 | 3.20 | 3/8 Sch 80S | 1.12 | - |
■
|
- | - | - |
21.3 | 2.65 | - | 1.24 |
■**
|
- | - | - |
■
|
21.34 | 2.11 | 1/2 Sch 10S | 1.01 | - | - |
■
|
- | - |
21.34 | 2.77 | 1/2 Sch 40S | 1.29 | - |
■
|
■
|
■
|
■
|
21.34 | 3.73 | 1/2 Sch 80S | 1.64 | - | - | - | - | - |
22 | 2 | - | 0.954 |
■
|
- | - | - | - |
26 | 4 | - | 2.20 |
■
|
- | - | - | - |
26.67 | 2.11 | 3/4 Sch 10S | 1.30 | - |
-
|
- | - | - |
26.67 | 2.87 | 3/4 Sch 40S | 1.71 | - |
■
|
■*
|
■*
|
■
|
26.67 | 3.91 | 3/4 Sch 80S | 2.18 | - |
■
|
-
|
-
|
-
|
26.9 | 2.65 | - | 1.61 |
■
|
- | - | - |
-
|
33.40 | 3.38 | 1 Sch 40S | 2.54 | - |
□
|
■*
|
□*
|
□
|
33.40 | 4.55 | 1 Sch 80S | 3.29 | - |
□
|
- | - |
□
|
33.7 | 3.25 | - | 2.48 |
□*
|
- | - | - |
□
|
38 | 5 | - | 3.93 | □ | - | - | - | - |
38 | 6.3 | - | 4.89 | - | ■ | - | - | - |
42.16 | 3.56 | 1¼ Sch 40S | 3.22 | - |
□*
|
□*
|
□
|
□
|
42.4 | 3.25 | - | 3.19 |
□*
|
- | - | - |
□
|
44.5 | 3 | - | 3.12 |
□*
|
- | - | - | - |
48.26 | 2.77 | 1½ Sch 10S | 3.15 | - |
□*
|
- | - | - |
48.26 | 3.68 | 1½ Sch 40S | 4.11 | - |
□*
|
□
|
□
|
□
|
48.26 | 5.08 | 1½ Sch 80S | 5.49 | - |
□
|
- | - |
□
|
48.3 | 3.25 | - | 3.67 |
□*
|
- | - | - |
□
|
50 | 9 | - | 8.89 | □ | □ | |||
60.3 | 3.65 | - | 5.18 |
□*
|
- | - | - |
□
|
60.33 | 2.77 | 2 Sch 10S | 3.99 | - |
□*
|
- | - | - |
60.33 | 3.91 | 2 Sch 40S | 5.52 | - |
□*
|
□
|
□
|
□
|
60.33 | 5.54 | 2 Sch 80S | 7.60 |
□
|
- | - | - |
□
|
60.33 | 10 | - | 12*** | □ | □ | - | - | - |
73.03 | 5.16 | 2½ Sch 40S | 8.77**** | - |
□
|
- | - |
□
|
76.1 | 3.65 | - | 6.62 |
□*
|
- | - | - |
□
|
88.9 | 4.05 | - | 8.60 |
□*
|
- | - | - |
□
|
88.90 | 5.49 | 3 Sch 40S | 11.5 | - |
□
|
□
|
- |
□
|
114.30 | 6.02 | 4 Sch 40S | 16.3 | - |
□
|
- | - |
□
|
168.28 | 7.11 | 6 Sch 40S | 28.7 | - |
□
|
- | - |
□
|
* Stocked in double random lengths
** Stocked in both standard random lengths and double random lengths
*** The weight for Sandvik 253 MA is 12.33 kg/m
**** The weight for Sandvik 253 MA is 8.973 kg/m.
Tolerances
Condition | Tolerance OD | Tolerance WT |
---|---|---|
Cold-worked | +/-0.75%, but min. +/- 0.3 mm (D3) |
+/-10% (T3), but min. +/- 0.2 mm |
Hot-worked | +/-1,5%, but min. +/- 0.75mm (D1) |
+/-5% (T1), but min. +/- 0.6 mm |
Size mm/condition | Tolerance OD, mm | Tolerance WT |
---|---|---|
Cold-worked 15.8-38.1 mm |
+/-0.19 | +/-0.10 |
Hot-worked | Tolerances according to ASTM A999, see table below for Sandvik 253 MA and 353 MA. |
OD, mm | Tolerance, mm |
---|---|
10.3-48.3 | +0.4/-0.8 |
(48.3-114.3) | +/-0.8 |
(114.3-219.1) | +1.6/-0.8 |
OD, mm | Tolerance, mm |
---|---|
10.3-48.3 | +0.4/-0.8 |
(48.3-114.3) | +/-0.8 |
(114.3-219.1) | +1.6/-0.8 |
Size, mm | WT, % | Thickness/OD ratio |
---|---|---|
10.3-48.3 | +20/-12.5 | All |
(48.3-114.3) | +22.5/-12.5 | Less or equal to 0.05 |
(114.3-219.1) | +15/-12.5 | Above 0.05 |
Product standards
Sandvik 4C54 (ASTM 446-1)
- ASTM A268 (tube)
- EN 10297-2
Sandvik 253 MA (UNS S30815)
Sandvik 353 MA (UNS S35315)
- ASTM A312 (pipe)
- EN 10297-2
Sanicro 31HT (UNS N08811/N08810)
- ASTM B407
Sandvik 7RE10 (UNS S31008/S31009, ASTM 310H/310S, EN 1.4845)
- ASTM A312/ASME SA312
- EN 10297-2
- EN 10216-5 TC1
- NACE MR0175/ISO 15156
* 253 MA and 353 MA are trademarks owned by Outokumpu OY.