Hollow bar grades (incl. nominal chemical composition)
Alleima grade UNS ASTM EN / W.nr. C Cr Ni Mo Others
Sanmac® 304/304L S30403/30400 304/304L 1.4301/1.4307 ≤0.030 18.5 9 - -
Sanmac® 316/316L S31603/31600 316/316L 1.4401/1.4404 ≤0.030 16.5 11 2.1 -
Sanmac® 4571 S31635 (316Ti) 1.4571 0.03 17 12.5 2.1 Ti
Sanmac® 2205 S32205/S31803 - 1.4462 ≤0.030 22.5 5.5 3.2 N