Tube, pipe, fittings and flanges
Scrubber tubes in stainless steel are used for the efficient production of urea. This portfolio includes Safurex, a material designed to enable an oxygenless process that increases both output and safety. Scrubber tubes from Alleima are supplied in accordance with the Stamicarbon specification.
Material | Description |
---|---|
Safurex* | Safurex is a patented, highly corrosion resistant material developed for the Stamicarbon process. It is designed to enable an oxygenless process that increases output and safety. |
Alleima® 2RE69 | Alleima® 2RE69 ("25.22.2") is developed specifically for the most severe conditions in the urea production process. It is a special high-alloy grade with a very low or zero ferrite content. |
* Contact us for more information