Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Pressurfect® CNG is a dual grade certified (ASTM 316/316L) austenitic chromium-nickel steel with minimum 2.5% molybdenum and a low carbon content used for compressed natural gas (CNG) fuel systems.

The grade is characterized by:

  • Excellent corrosion resistance in CNG environments
  • Excellent toughness
  • Excellent bendability
  • Excellent impact strength

Standards

  • ASTM: TP316L, TP316
  • UNS: S31603, S31600
  • EN Number: 1.4435, 1.4436
  • EN Name: X 2 CrNiMo 18-14-3, X 3 CrNiMo 17-13-3
  • JIS: SU316LTP, 316TP, SU316LTB, 316TB

Product standards

  • ASTM A213, A269 and A312
  • JIS G3459
  • JIS G3463
  • EN 10216-5

Product Approval
JIS Approval No. SE9402 for Stainless Steel Tubes

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.