Sanicro® 625

Tube and pipe, seamlessDatasheet

Datasheet updated 2019-12-13 14:38 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 625 is an austenitic nickel-chromium alloy characterized by:

  • Extremely good corrosion resistance in widely varying acidic and chloride containing environments
  • High strength
  • Excellent fabrication properties.

Sanicro® 625 can be used in a wide range of temperatures from -196°C to 815°C (-321°F to 1500°F). Typical uses include hydraulic and instrumentation systems, heat-exchangers and high-temperature applications. However, it should be noted that prolonged exposure to temperatures above 600°C (1100°F) may lead to embrittlement.

Standards

  • UNS: N06625
  • ISO: NW6625

Product standards

ASTM B444, Grade 1 and Grade 2
ASME SB444, Grade 1 and Grade 2
ISO 6207

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email