Selected maraging steels incl. chemical composition (nominal), %
Alloy Hardness (heat treated condition), HRC Fe C Mn Si Cr Ni Mo Co Ti Al
18Ni300 52 Bal. 0.03* 0.1* 0.1* 0.3* 18.0 4.8 9.0 0.7 0.1
1.2709 54 Bal. 0.03* 0.1* 0.1* - 18.0 5.2 9.5 0.9 -

*Maximum value