Unions, socket weld

Tube, pipe, fittings and flanges

ASTM A182 3000 lbs ASME B16.11 / BS 3799, MSS SP-83

Product code example:

FSU-316L-1-3000

● = stock standard

3711-[Converted].png
B L1 L Weight ASTM ASTM
in. mm socket mm (nom.) ~kg/pce 304/304L 316/316L
1/4
3/8
1/2
3/4
14.20
17.60
21.80
27.20
9.53
9.53
9.53
12.50
44.4
46.0
49.0
56.9
0.20
0.35
0.40
0.45






1


2
33.90
42.70
48.80
61.20
12.50
12.50
12.50
16.00
62.0
71.1
76.5
86.1
1.00
1.30
1.70
3.00