Sandvik titanium tubing is available in size range outside diameter 9.53–38.1 mm (3/8–1½ in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.). The titanium tubes tubes are delivered in straight lengths or as U-bent tubes.
Grades and standards
Sandvik grade | UNS | ASTM/ASME | W.Nr. | AFNOR |
---|---|---|---|---|
Ti Grade 1 (CP Ti) | R50250 | Grade 1 | W.Nr. 3.7025 | T-35 |
Ti Grade 2 (CP Ti) | R50400 | Grade 2 | W.Nr. 3.7035 | T-40 |
Ti Grade 3 (CP Ti) | R50550 | Grade 3 | W.Nr. 3.7055 | T-50 |
Ti Grade 7 | R52400 | Grade 7 | W.Nr. 3.7235 | - |
Ti Grade 9 | R56320 | Grade 9 | W.Nr. 3.7195 | T-A3V2.5 |
Ti Grade 11 | R52250 | Grade 11 | W.Nr. 3.7225 | - |
Ti Grade 12 | R53400 | Grade 12 | W.Nr. 3.7105 | - |
Ti Grade 16 | R52402 | Grade 16 | - | - |
Ti Grade 17 | R52252 | Grade 17 | - | - |
Ti Grade 26 | R52404 | Grade 26 | - | - |
Ti Grade 28 | R52254 | Grade 28 | - | - |
Sandvik grade | Description |
---|---|
Ti Grade 1 (CP Ti) | Relatively low-strength and high-ductility pure titanium (Cp). |
Ti Grade 2 (CP Ti) | Medium-strength pure titanium (Cp). |
Ti Grade 3 (CP Ti) | High strength pure titanium (Cp). |
Ti Grade 7 | Medium-strength Pd-alloyed titanium for enhanced corrosion properties. |
Ti Grade 9 | High-strength titanium alloyed with 3% Al and 2.5% V. |
Ti Grade 11 | Low-strength titanium plus 0.12-0.25% Pd for enhanced corrosion properties. |
Ti Grade 12 | High-strength titanium alloy plus 0.3% Mo and 0.8% Ni for enhanced corrosion properties. |
Ti Grade 16 | Medium-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties. |
Ti Grade 17 | Low-strength titanium plus 0.04-0.08% Pd for enhanced corrosion properties. |
Ti Grade 26 | Medium-strength titanium plus 0.08-0.14% Ru for enhanced corrosion properties. |
Ti Grade 28 | High-strength titanium alloy plus 3% Al, 2.5% V and 0.08%-0.14% Ru for enhanced corrosion properties. |
Type of product | Grade(s) | Technical requirements* according to |
---|---|---|
Titanium tubes and pipes | Ti and Ti alloy grades 1, 2, 3, 7, 9, 11, 12, 16, 17, 26 and 28 | ASTM B337, ASTM B338, ASME SB338 NACE MRO 175-94 VdTÜV 230/2 Dimensional tolerances acc. to DIN 17861 D3/T3 or closer |
*Other requirements on request
Mechanical properties
Sandvik grade | UNS | Proof strength Rp0.2 MPa min | Tensile strength Rm MPa min | Elongation A % min |
---|---|---|---|---|
Cp Ti Grade 1 | R50250 | 138-310 | 240 | 24 |
Cp Ti Grade 2 | R50400 | 275-450 | 345 | 20 |
Cp Ti Grade 3 | R50550 | 380-550 | 450 | 18 |
Ti Grade 7 | R52400 | 275-450 | 345 | 20 |
Ti Grade 9 | R56320 | 483 | 620 | 15 |
Ti Grade 11 | R52250 | 138-310 | 240 | 24 |
Ti Grade 12 | R53400 | 345 | 483 | 18 |
Ti Grade 16 | R52402 | 275-450 | 345 | 20 |
Ti Grade 17 | R52252 | 138-310 | 240 | 24 |
Ti Grade 26 | R52404 | 275-450 | 345 | 20 |
Ti Grade 28 | R52254 | 483 | 620 | 15 |
Sizes and tolerances
Sizes and tolerances for titanium tubes
Sandvik titanium tubes are available in size range outside diameter 9.53-38.1 mm (3/8 - 1 1/2 in.) with wall thicknesses from 0.7 to 5 mm (0.0275 to 0.1968 in.)*.
OD = outside diameter
WT = wall thickness
Size OD, mm (in.) | Tolerances OD, mm (in.) | WT min wall % |
---|---|---|
< 25.4 (< 3/8) | ±0.102 (0.004) | +20/-0 |
25.4-38.1 (1-1 1/2) | ±0.127 (0.005) | +20/-0 |
Tolerances for OD < 15.9 or > 38.1 - or closer tolerances - after special agreement.
*Limitations for some ratios of OD/WT exist
Type of product | Grade(s) | Technical requirements |
---|---|---|
Titanium tubes and pipes | Ti and Ti alloy grades: 1, 2, 3, 7, 9, 11, 12, 16, 17, 26, 28 and 29 | ASTM B337, ASTM B338, ASME SB338 NACE MRO 175-94 VdTÜV 230/2 Dimensional tolerances acc. to DIN 17861 D3/T3 or closer |
Lengths
Titanium tubes are delivered in straight lengths up to 16.5 meters (54 ft). U-bent tubes are available on request.