Umbilical tubes

Sandvik is a market leader in stainless steel umbilical tubing. Since the mid-1990s, we have supplied more than 100 million meters (or 330 million feet) of umbilical tubes to all major fabricators and oil companies in all offshore regions. Our umbilical tubes are used in all offshore regions.

Need to know more?

Call us Email us

Coiled tubing for cost-effective umbilical manufacturing

Sandvik offers orbital-welded coiled tubing for cost-effective umbilical manufacturing. Our umbilical tubes are also offered in straight lengths, as long as 40 meters (131 feet), for a minimum requirement of orbital welds.

Umbilical tube materials

SAF 2507® (UNS S32750)
A super-duplex stainless steel that combines high corrosion resistance and high mechanical strength. With excellent resistance to seawater and marine environments, it is particularly well-suited for applications exposed to high stress in aggressive chloride-rich environments. The resistance to sour environments is superior to SAF 2205™ (UNS S31803/S32205). PRE value min. 42.5 (valid for tube and pipe).
Read more about SAF 2507®
SAF 3207 HD™ (UNS 33207)
A hyper-duplex stainless steel developed for deepwater umbilicals. It is designed for the most extreme conditions in terms of depth, temperature and pressure. SAF 3207 HD™ offers greater yield strength, greater corrosion resistance and superior fatigue properties compared to super-duplex stainless steels. PRE value min. 50 (valid for tube and pipe).
Read more about SAF 3207 HD™

Size range

Coiled and straight tubes
Inner diameter Wall thickness (mm)
in. mm min max
3/8 9.53 1.2 2
1/2 12.70 1 2.6
5/8 15.88 1 3
3/4 19.05 1.1 4
1 25.40 1.3 5
31.75 1.5 5
38.10 2
44.45 2.5 5.5 1)
2
50.80 2.7 6 1)

1) Specific NDT acceptance criteria are applied for these dimensions

Straight tubes only

Inner diameter Wall thickness (mm)
in. mm min max
44.45 2.50 8.00
2 50.80 2.80 8.00
57.15 3.20 9.00
63.50 3.50 8.00
69.85 4.00 8.00
3 76.20 4.30 10.00
82.55 4.60 8.00
88.90 4.90 12.00
95.25 5.30 9.00
4 101.60 5.50 14.00
114.30 6.30 16.00
5 127.00 7.00  18.00

Duplex stainless steels

Sandvik's range of duplex stainless steels is the widest on the market. The range includes super-duplex and hyper-duplex stainless steels.
Read more about duplex stainless steels