Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 20C is a hardened and tempered carbon steel used for shock absorber shims. Sandvik 20C shock absorber steel is characterized by:

  • High strength and wear resistance
  • High fatigue strength under bending and impact stress
  • Excellent surface finish
  • Low level of non-metallic inclusions
  • Good dimensional tolerances
  • Good flatness

Standards

  • ASTM: 1095
  • EN Number: 1.1274

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.