Blooms

Billets and blooms

Continuous cast blooms for the production of strip, wire, bar, hexagons and profiles. Concast blooms from Alleima are characterized by very fine surface finish and available in a wide range of stainless steels, including duplex steels. Electromagnetic stirrers ensure a homogenous structure.

View list of materials

Blooms
Standard program - blooms
Size range,
mm (in.)
Tolerances,
mm (in.)
Lengths,
m (ft)
Surface condition
150 x 150
(5.90 x 5.90)
± 5 (±0.1968) 5 – 7
(16.4 – 23)
As cast
265 x 265
(10.43 x 10.43)
± 5 (±0.1968) 1.5 – 6
(4.9 – 19.7)
As cast
265 x 365
(10.43 x 14.37)
± 5 (±0.1968) 1.5 – 6
(4.9 – 19.7)
As cast