Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R60™ Urea Grade is a high-purity variant of ASTM 316L, specially developed for the urea industry. The grade has a guaranteed maximum ferrite content of 0.6%. Sandvik 3R60™ Urea Grade is characterized by:

  • High resistance to corrosion in ammonium carbamate
  • High resistance to intergranular corrosion
  • Good weldability

Standards

  • ASTM: TP316L
  • UNS: S31603
  • EN Number: 1.4435
  • EN Name: X 2 CrNiMo 18-14-3
  • W.Nr.: 1.4435
  • DIN: X 2 CrNiMo 18 14 3
  • SS: 2353
  • BS: 316S13

Urea specifications issued by
Stamicarbon
Snamprogetti
Urea Casale
Kellogg

Product standards
ASTM A213, A312
EN 10216-5
DIN 17458

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.