Sandvik knife steels

The Sandvik program includes knife steel for all types of knives. Our knife steel is used in, for example, kitchen knives, chef's knives, fishermen's knives, hunting knives, folding knives and different types of industrial knives.
Every Sandvik knife steel has its benefits, ranging from excellent corrosion resistance to extreme hardness. The application determines the requirements of the knife. Choose a knife steel for your particular application and read more about its specific benefits.
Sandvik knife steels
- Sandvik 14C28N - Combination of hardness and corrosion resistance
- Sandvik 7C27Mo2 – High corrosion resistance
- Sandvik 12C27 – The well-rounded knife steel
- Sandvik 12C27M – Dish washer safe
- Sandvik 13C26 – Razor edge sharpness
- Sandvik 19C27 – Excellent wear resistance
- 10C28Mo2
- 10C16Mo3V1
* For electric shavers
Material selection table
Type of knife /application | Sandvik 6C27 |
Sandvik 7C27Mo2 |
Sandvik 12C27 |
Sandvik 12C27M |
Sandvik 13C26 |
Sandvik 14C28N |
Sandvik 19C27 |
Sandvik 10C16Mo3V1 | Sandvik 10C28Mo2 |
---|---|---|---|---|---|---|---|---|---|
Bread knives | - | - |
■
|
- | - | - | - | - | - |
Butcher's knives | - | - |
■
|
- | - | - | - | - | ■ |
Carpet knives | - | - | - | - | ■ | - |
■
|
■
|
-
|
Carving knives | - | - |
■
|
- | - | - | - | - | - |
Chef's knives | - | - |
■
|
- | - | ■ | - | - | ■ |
Circular knives |
■
|
■
|
■
|
■
|
■
|
- | - | - | - |
Cutting heads* | ■ | - | - | - |
■
|
- | - | - | - |
Fishermen's knives | - |
■
|
■
|
- | - | ■ | - | - | ■ |
Folding knives | - | - |
■
|
- | - |
■
|
- | - | ■ |
Frying slicers (spatulas) | ■ | - | - | - | - | - | - | - | - |
Hunting knives | - | - |
■
|
- | - | - | - | - | ■ |
Ice drills | - | - |
■
|
- | - | - | - | - | - |
Industrial knives | - |
■
|
- | - |
■
|
- |
■
|
■
|
-
|
Kitchen knives | - | - |
■
|
■
|
- | - | - | - | ■ |
Paper knives | - | - | - | - |
■
|
- | ■ | - | - |
Plastic film knives | - | - | - | - | ■ | - | ■ | - | - |
Pocket knives | - | - |
■
|
- | - | ■ | - | - | ■ |
Pruning shears | - | - |
■
|
- | - | - | - | ■ | - |
Shaver knives* | - |
■
|
- | - | - | - | - | - | - |
Skate blades | - | - |
■
|
- | - | - | - | - | - |
Surgical knives | - | - | - | - | ■ | - | - | - | - |
Synthetic fibre knives | - | - | - | - |
■
|
- |
■
|
-
|
-
|
Trimmers* | ■ | - | - | - |
■
|
- | - | - | - |
* For electric shavers