End caps, NPT-threaded

Need to know more?

Call us Email us

ASTM A182 3000 lbs, ASME B16.11 / BS 3799

Product code example:

FTCAP-316L-1/4-3000

● = stock standard

Nominal pipe size L D G
Weight
ASTM
in. mm mm mm ~kg/pce 316/316L
1/4
3/8
1/2
3/4
25.4
25.4
31.8
36.5
19.1
22.2
28.6
34.9
4.76
4.76
6.35
6.35
0.05
0.06
0.12
0.19



1
1 ¼
1 ½
2
41.3
44.5
44.5
47.6
44.5
57.2
63.5
76.2
9.53
9.53
11.11
12.70
0.35
0.56
0.75
1.45