Unions, NPT-threaded

Need to know more?

Call us Email us

ASTM A182 3000 lbs, ASME B16.11 / BS 3799, MSS SP-83

Product code example:

FTU-316L-1-3000

● = stock standard

Nominal pipe size L A
Weight
ASTM
ASTM
in. mm (min.) mm ~kg/pce 304/304L 316/316L
1/4
3/8
1/2
3/4
41.4
46.0
49.0
56.9
19.0
22.9
27.7
33.5
0.13
0.20
0.40
0.50






1
1 ¼
1 ½
2
62.0
71.1
76.4
86.1
44.4
50.5
57.2
70.1
1.00
1.45
1.60
2.50