High-pressure tubes

Tube, pipe, fittings and flanges

Seamless high-pressure tubes for a variety of high-pressure applications using liquid or gas as the pressure medium, such as hydraulic installations, test benches and water-jet cutting equipment.

High-pressure tubes

High-pressure tubes from Alleima are characterized by high yield strength and high tensile strength in combination with high elongation. The pressure resistance is guaranteed by the very smooth inside surface. An autofrettage treatment prolongs the cycle fatigue behavior.

Grades and standards
Alleima grade UNS ASTM EN steel no. W.Nr. AFNOR
Alleima® 5R10 S30400 304 1.4301 1.4301 Z2CND18-09
Alleima® 3R65 S31603/S31600 316L/316 1.4404/1.4401 1.4404 Z2CND17-12
SAF™ 2507 S32750
-
1.4410
-
-
Alleima HP160*
-
-
-
-
-
Alleima® 254 SMO S31254 - - - Z1CNDU20-18-06AZ

* Contact us for more information

Mechanical properties
Alleima grade Yield strength
Rp0,2 min. MPa
Tensile strength
Rm min. MPa
Elongation A
%, min
Alleima® 5R10 1) 600 700 18
Alleima® 3R65 1) 600 700 18
SAF™ 2507 2) 550 800-1,000 25
Alleima HP160* 2) 450 850 35
Alleima® 254 SMO 2)  340 650 65 

1) Hard condition.
2) Annealed condition. Tubes with higher values can be offered on request.
* Contact us for more information