Tube, pipe, fittings and flanges
Seamless high-temperature tubes and furnace tubes suitable for use in applications with temperatures above 500ºC (932ºF).
The Alleima portfolio of high-temperature tubes includes a wide range of austenitic stainless steels and nickel alloys as well as iron-chromium-aluminium (FeCrAl) alloys, which can be used at temperatures up to 1250ºC (2280ºF).
|
|
Alleima holds stock of five different grades commonly used in a variety of high-temperature tube applications. We also stock composite tubes.
View stock program of high-temperature tubes
View stock program of radiant tubes in FeCrAl alloys
Alleima grade | UNS | ASTM | EN steel no. |
---|---|---|---|
Alleima® Esshete 12501) | S21500 | - | 1.4982 |
Alleima® 5R10 | S30400/S30409 | 304/304H | 1.4301/1.4948 |
Alleima® 253 MA2) | S30815 | - | 1.4835 |
Alleima® 8RE18 | S30908/30909 | 309S, 309H | 1.4833 |
Alleima® 7RE10 | S31008/S31009 | 310S, 310H | 1.4845 |
Sanicro® 253) | S31035 | - | - |
Alleima® 6LR62 | S31600/S31609 | 316, 316H | 1.4401 |
Alleima® 8R61 | - | ASTM (316H) | 1.4918 |
Alleima® 6R35 | S32100/S32109 | 321/321H | 1.4541/1.4940 |
Alleima® 8R40 | S34700/S34709 | 347/347H | 1.4550/1.4912 |
Alleima® 6R44 | S34700/S34709 | 347/347H | 1.4550/1.4912 |
Alleima® 8R41 | - | - | 1.4961 |
Alleima® 353 MA2) | S35315 | - | 1.4854 |
Alleima® 2C48 | S44600 | 446-2 | - |
Alleima® 4C54 | S44600 | 446-1 | 1.4749 |
Sanicro® 625 | N06625 | Alloy 625 | - |
Sanicro® 61 | N06601 | - | - |
Sanicro® 70 | N06600 | Alloy 600 | - |
Sanicro® 31H4) | N08810 | Alloy 800H | 1.4958 |
Sanicro® 31HT | N08811/N08810 | - | 1.4959 |
Kanthal APM | - | - | - |
Kanthal APMT | - | - | - |
1) Esshete 1250 is a trademark owned by Corus
2) 253 MA and 353 MA are trademarks owned by Outokumpu OY
3) Approved as per Vd TÜV 555
4) Contact us for more information
Alleima grade | UNS | ASTM/ ASME |
EN steel no. | EN steel name |
---|---|---|---|---|
Corrosion-resistant alloys | ||||
Sanicro® 67 | N06690 | - | 2.4642 | - |
Sanicro® 38 | N08825 Mod. | - | 2.4858 | - |
Sanicro® 30 | N08800 | - | 1.4558 | - |
Sanicro® 28 | N08028 | - | 1.4563 | X1NiCrMoCu31-27-4 |
Alleima® 3RE28 | - | 310 | 1.4845* | - |
Alleima® 3R12 | S30403/ S30400 |
304L | 1.4306 | - |
Load-carrying alloys, pressure-bearing components | ||||
4L7 | - | SA210-A1 (C) | 1.0425 | P265GH |
3Mo1 | - | - | 1.5415 | 16Mo3 |
HT5 | - | SA213-T12 | 1.7335 | 13CrMo4-5 |
HT8 | - | SA213-T22 | 1.7380 | 10CrMo910 |
T23 | SA213-T23 | 1.8201 | 7CrWVMoNb9-6 | |
T24 | - | SA213-T24 | 1.7378 | 7CrMoVTiB10-10 |
HT7 | - | SA213-T91 | 1.4903 | X10CrMoVNb9-1 |