Sandvik Santronic pre-coated strip steel for electronic components is available with the following coating.

Need to know more?

Call us Email us

Coating Coating characteristics
Nickel (Ni) Good corrosion resistance, good electrical conductivity, good fatigue properties (in high strength condition).

* Other coatings are available on request

Tailor-making and new applications

Sandvik flexible coating process allows for unique possibilities to combine coatings on both sides.