Sandvik SAF 2707 HD

Sandvik SAF 2707 HD is Sandvik's trademark for a hyper-duplex stainless steel characterized by excellent resistance to stress corrosion cracking (SCC), pitting and crevice corrosion, high resistance to general corrosion and very high mechanical strength.

Sandvik SAF 2707 HD hyper-duplex steel is available as a tube product. Specially developed welding consumable for Sandvik SAF 2707 HD is Sandvik 27.7.5.L welding wire.

Product advantages

Read about the benefits of using tube in Sandvik SAF 2707 HD.

Material datasheets

Related material datasheets

Related products

Tube and pipe in seamless and welded condition, fittings and flanges.

Slicklines and armor wire for logging cables in a wide range of stainless steels and high-alloyed materials.