Sandvik’s welding consumables business has been acquired by ESAB from February 1, 2018. Over the coming months ESAB will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik welding products will continue to be accessible on this website, or via the ESAB website.

ESAB Website

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Sandvik AWS A5.11 ISO 14172 W.Nr.
Sanicro® 53 ENiCrCoMo-1 ENi6117 2.4663
Sanicro® 54 ENiCrMo-10 ENi6022 2.4602
Sanicro® 56 ENiCrMo-4 ENi6276 2.4819
Sanicro® 59 ENiCrMo-13 ENi6059 2.4605
Sanicro® 60 ENiCrMo-3 ENi6625 2.4856
Sanicro® 69 ENiCrFe-7 ENi6152 2.4627
Sanicro® 71 ENiCrFe-3 ENi6182 2.4807