Sandvik’s welding consumables business has been acquired by ESAB from February 1, 2018. Over the coming months ESAB will be integrating the Sandvik portfolio, to provide a smooth transition for customers. During the integration period, the full line of Sandvik welding products will continue to be accessible on this website, or via the ESAB website.

ESAB Website

Flux cored welding electrodes in a variety of grades and sizes for flat, horizontal or all-position welding.

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Sandvik gradeAWS A5.22ISO 17633
W.Nr.
19.9.L T0 E308LT0-1/T0-4 T 19 9 L R C 3/T 19 9 L R M 3 1.4316
19.9.L T1 E308LT1-1/T1-4 T 19 9 L P M 1 1.4316
19.9.H T1 E308HT1-1/T1-4 - 1.4316
19.9.Nb T1 E347T1-1/T1-4 - 1.4551
19.12.3.L T0 E316T0-1/T0-4 T 19 12 3 L R C 3/T 19 12 3 L R M 3 1.4430
19.12.3.L T1 E316T1-1/T1-4 T 19 12 3 L P M 2 1.4430
19.13.4.L T0 E317T0-1/T0-4 - 1.4438
19.13.4.L T1 E317T1-1/T1-4 - 1.4438
22.9.3.L T1 E2209T1-1/T1-4 T 22 9 3 N L P C M 2 1.4462
23.12.2.L T0 E309LMoT0-1/T0-4 T 23 12 2 L R C M 3 1.4333
23.12.2.L T1 E309LMoT1-1/T1-4 T 23 12 2 L R C M 1 1.4333
24.13.L T0 E309LT0-1/T0-4 T 23 12 L R C 3/T 23 12 L R M 3 1.4332
24.13.L T1 E309LT1-1/T1-4 T 23 12 L R C 2/T 23 12 L P M 2 1.4332
25.10.4.L T1 E2594T1-1/T1-4 - 1.4410
29.9. T1 E312T1-1/T1-4 - 1.4337