Sandvik produces steam generator tubes that meet the most stringent Eddy Current Multi Frequency Inspection demands and a signal-to-noise ratio of 15:1 or better. The tubes are manufactured in a mill specially designed for production of long U-bent steam generator tubes, with state-of-the-art non destructive examination (NDE) equipment.