Sandvik provides Safeni™ 52, a soft magnetic iron-nickel (FeNi) alloy wire for reed switches. Safeni™ 52 soft magnetic wire offers reed switch producers a range of product benefits that contribute to high material yields, increased productivity and reed switch reliability.

Safeni™ 52 soft magnetic wire for reed switches is characterized by, for example:

  • High and consistent surface quality for optimum wire coating, clean running and wire-to-glass sealing in reed switch production
  • Excellent straightness for high production feeds and throughput rates
  • Maximized magnetic properties for end-product reliability and long reed switch life
  • Thermal expansion compatibility with borosilicate glass for glass-to-metal sealing

Safeni™ 52 is also available as strip.