New alloys, new certifications, same high precision standards

To open up new possibilities for you, we continue to expand our range of solutions for extreme thick-walled tubing (1-70 mm OD) as well as high pressure (up to 160,000 psi) and ultra-pure tubing for some of the world’s most demanding applications.

Nickel alloys 625 and C276

For hydraulic and instrumentation tubing, we’re now qualified to provide nickel alloy tubing in Alloy 625 (UNS N06625) / Sanicro 625 and Alloy C276 (UNS N10276) / Sanicro 56. These grades are well suited to combat aggressive hot chloride-containing environments.

Green Factory. NORSOK. DIN EN 9100

Our high-precision tube plant has now received certification ISO 50001 (Energy Management), an important step in realizing our Green Factory concept. NORSOK approvals for the oil and gas sector as well as DIN EN 9100 certification for the aerospace industry have been granted.

Read more about our thick wall precision tubing products