SAF 2205™+

BarDatasheet

Datasheet updated 2021-10-07 11:05 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

SAF 2205™+ is a duplex (austenitic-ferritic) stainless steel with excellent material cleanliness, for highly demanding applications. The grade is characterized by:

  • Alignment to IOGP S-563 and ISO 17781 standards
  • Decreased phosphorous and sulfur content to match higher demanding applications
  • High resistance to stress corrosion cracking (SCC) in chloride-bearing environments
  • High resistance to stress corrosion cracking (SCC) in environments containing hydrogen sulphide
  • High resistance to general corrosion, pitting and crevice corrosion
  • High mechanical strength – roughly twice the proof strength of austenitic stainless steels
  • Good hot-working properties
  • High resistance to erosion corrosion and corrosion fatigue
  • Physical properties that offer design advantages
  • Good weldability

Standards

  • UNS: S31803, S32205
  • EN Number: 1.4462
  • W.Nr.: 1.4462

Product standards

  • IOGP S-563:2018
  • ISO 17781:2017
  • EN 10088-3, EN 10088-5 (dimensions up to 160 mm), EN 10272, EN 10222-5,
  • ASTM A479, ASTM A276,
  • NORSOK MDS D47 Rev 3, Rev 4, Rev 5 
  • Chemical composition and mechanical properties acc. to ASTM A182

Approvals

  • Pressure Equipment Directive (PED 2014/68/EU)
  • NORSOK M650 Ed. 4, NORSOK M630 Ed. 6, dimensions up to 260 mm.
  • DNV, dimensions up to 300 mm
  • Pre-approval for PMA

Certificate

  • Status according to EN 10204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.