Sanmac 329

BarDatasheet

Datasheet updated 2019-06-19 15:06 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac 329 is a duplex stainless steel with optimized sulfur content and inclusion morphology for improved machinability. The grade is characterized by:

  • Excellent machinability
  • High mechanical strength
  • Very good resistance to pitting and stress corrosion cracking

    Standards

    • EN Number: 1.4460

    Product standard

    • EN 10088-3

    Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.