Sandvik 10RE51

Hollow barDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 10RE51 is a duplex (austenitic-ferritic) stainless steel characterized by resistance to stress corrosion cracking (SCC), high resistance to pitting, crevice and general corrosion and very high mechanical strength.

Standards

  • UNS: S32900
  • EN Number: 1.4460

Product standards

EN 10297-2, EN 10294-2, ASTM A790

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email