Sanbar® 64

Hollow drill steelDatasheet

Datasheet updated 2018-07-05 08:57 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanbar® 64 is an air-hardening, high nickel alloy steel with good response to carburizing. It has excellent fatigue strength and wear resistance in the case hardened condition.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.