Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 254 SMO* (ESR) is a high-alloy austenitic stainless steel developed for use in seawater and other aggressive chloride-bearing media. The steel is electroslag remelted which gives a cleaner material free from segregations. The grade is characterized by:

  • Excellent resistance to pitting and crevice corrosion
  • High resistance to general corrosion
  • High resistance to stress corrosion cracking
  • Higher strength than conventional austenitic stainless steels
  • Good weldability

Trademark information: 254 SMO is a trademark owned by Outokumpu OY.

Standards

  • UNS: S31254
  • EN Number: 1.4547
  • SS: 2378

Product standards

EN 10088-3

Suitable for production of flanges etc. according to ASTM A182 Grade F44.

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.