Sandvik 3R64

BilletsDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R64 is an austenitic stainless steel with a high molybdenum content. Significant properties, such as general and pitting corrosion resistance, are improved, in comparison with ASTM 316L.

sentence correction

Standards

  • ASTM: 317L
  • UNS: S31703
  • EN Number: 1.4438
  • W.Nr.: 1.4438
  • SS: 2367
  • BS: 317S16

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. according to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.