Sandvik 6LR11

BilletsDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6LR11 is an austenitic stainless chromium-nickel steel.

Standards

  • ASTM: 304
  • UNS: S30400
  • EN Number: 1.4301
  • W.Nr.: 1.4301
  • DIN: X 5 CrNi 18 10
  • SS: 2333
  • AFNOR: Z6CN18-09
  • BS: 304S31

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. according to ASTM A-182 Grade F304

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.