Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6LR62 is a molybdenum-alloyed austenitic stainless chromium-nickel steel.

Standards

  • ASTM: 316, 316H
  • UNS: S31600, S31609
  • EN Number: 1.4401
  • EN Name: 1.4401
  • AFNOR: Z7CND 17-11-02
  • BS: 316S31

Product standard

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. according to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email