Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 6RA11 is an austenitic stainless free-machining steel with addition of sulphur.

Standards

  • ASTM: 303
  • UNS: S30300
  • EN Number: 1.4305
  • W.Nr.: 1.4305

Product standards

  • EN 10088-3
  • ASTM A-314

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.